Secondary sealant in insulated glass units (IGUs)
The secondary sealant in insulated glass units (IGUs) plays a critical role in maintaining the unit’s integrity and performance.
=> Purposes:
1. Moisture Barrier:
- Moisture can fog up the IGU by condensing on the colder inner glass surface, reducing visibility and thermal insulation.
- Moisture can also corrode the metal spacer bar over time, leading to seal failure and potential gas leakage.
- The primary function of the secondary sealant is to create a watertight seal around the spacer bar, which separates the glass panes within the IGU.
- This prevents moisture from entering the airspace between the panes.
2. Gas Preservation:
- Insulated glass units are often filled with inert gases like argon gas or krypton gas to improve thermal insulation.
- These gases have lower thermal conductivity than air, reducing heat transfer through the window.
- The secondary sealant acts as a barrier, preventing these insulating gases from leaking out of the IGU.
- This maintains the unit’s thermal efficiency over its lifespan.
3. Structural Support (in Specific Applications):
- In some applications, particularly structural glazing, the secondary sealant may also contribute to the structural integrity of the window system.
- This typically involves using a strong silicone sealant that can bond the outer glass pane of the IGU to the building frame.
- However, this is not the primary function of the secondary sealant in most standard IGU applications.
=> The two-part sealant components:
The two-part sealants used for secondary sealing in insulated glass units typically consist of a base and a curing agent
- Base: This is usually a viscous paste containing Silicone or Polysulfide.
- It’s the main body of the sealant and provides properties like adhesion, flexibility, and weather resistance.
- Curing agent: This is often a paste or liquid that triggers the curing process when mixed with the base.
=> Mixing and Curing:
- By mixing the base and the curing agent in a specific ratio (10:1 to 14:1 base to Curing agent), a chemical reaction is initiated.
- This cures the sealant, transforming it from a paste-like state to a solid, rubbery form.
- Too little curing agent can lead to an Incomplete cure, weak and inflexible seal, and shortened lifespan.
- Too much curing agent can lead to a Potentially faster cure (may not be desirable), and possible waste of material. You can check for the suitable mixing ratio by Snap time test
- The color distinction between the base and curing agent helps ensure proper mixing.
- Seeing streaks of black or white during application indicates incomplete mixing, which can affect the sealant’s final properties. You can check that by butterfly test.