Troubleshooting SGCC Laminated Glass Ball Drop Test Failures – ASTM F3007 Help
<strong data-start=”384″ data-end=”466″>Troubleshooting SGCC Laminated Glass Ball Drop Test Failures – ASTM F3007 Help
We’ve been running into a frustrating issue at our facility and are hoping someone in the community has dealt with this or can offer insight.
We’re currently performing in-house ball drop impact testing on laminated glass according to ASTM F3007-13, as part of SGCC production testing requirements. This test uses a 2.3 kg (5 lb) steel ball dropped from 3.66 meters (12 feet) for Class A products.
The issue is that our in-house ball drop tests are consistently failing — either complete penetration or post-breakage retention failure. However, when we send the same laminated glass batch out for third-party testing to meet <strong data-start=”1095″ data-end=”1115″>CPSC 16 CFR 1201, which uses a <strong data-start=”1130″ data-end=”1162″>100 lb pendulum bag impactor, it passes.
We realize these are <strong data-start=”1197″ data-end=”1220″>two different tests — one for SGCC (ASTM F3007) and one for CPSC safety glazing — but we’re surprised that glass which passes the more severe-seeming CPSC bag test could fail the ball drop test.
<strong data-start=”1397″ data-end=”1452″>Here’s how we’re performing our in-house SGCC test:
<ul data-start=”1454″ data-end=”1787″>
2.3 kg (5 lb), 83 mm smooth steel ball
Drop height: 3.66 m (12 ft ± 5 in)
Glass conditioned for 4+ hours at 24°C ± 5°C (75°F ± 9°F)
Support frame built by SGCC we purchased their recommended ball drop
Light clamping or no clamping, but unsure if that’s affecting results
Testing the thinnest configuration from the batch
<strong data-start=”1789″ data-end=”1818″>Things we’re questioning:
<ul data-start=”1820″ data-end=”2101″>
Is our drop height or release inconsistent?
Could our ball surface be worn or damaged?
Is the clamping or support method introducing extra stress?
Are environmental conditions during testing affecting results?
Could EVA cure variation be impacting break behavior?
<strong data-start=”2103″ data-end=”2128″>Looking for feedback:
Has anyone else seen this kind of inconsistency between passing third-party CPSC impact tests and failing in-house SGCC ball drop tests?
We’d appreciate any tips on:
<ul data-start=”2297″ data-end=”2530″>
How to properly set up a compliant ASTM F3007 drop test
How much clamping is too much
Whether you’ve seen EVA-based lami act unpredictably in ball drop tests
Whether test rig calibration or support surfaces have played a role
Sorry, there were no replies found.
Log in to reply.