Troubleshooting SGCC Laminated Glass Ball Drop Test Failures – ASTM F3007 Help
<b data-start=”380″ data-end=”476″>Troubleshooting In-House Failures – Ball Drop Test (ASTM F3007 / SGCC Production Testing)
Hi everyone,
We’ve been running into a frustrating issue at our facility and are hoping someone in the community has seen this before or can offer some insight.
We’re currently performing <strong data-start=”668″ data-end=”705″>in-house ball drop impact testing on laminated glass per <strong data-start=”729″ data-end=”746″>ASTM F3007-13 as part of <strong data-start=”758″ data-end=”798″>SGCC production testing requirements. We’re using the standard <strong data-start=”825″ data-end=”853″>2.3 kg (5 lb) steel ball dropped from <strong data-start=”867″ data-end=”892″>3.66 meters (12 feet) for <strong data-start=”897″ data-end=”908″>Class A products.
Here’s the problem:<br data-start=”939″ data-end=”942″> When we send the <strong data-start=”959″ data-end=”995″>exact same laminated glass batch to an <strong data-start=”1002″ data-end=”1021″>independent lab, it <strong data-start=”1026″ data-end=”1036″>passes. But when we test in-house, we’re consistently seeing <strong data-start=”1091″ data-end=”1103″>failures — either complete penetration or glass not meeting post-breakage retention.
<hr data-start=”1181″ data-end=”1184″>
<b data-start=”1186″ data-end=”1208″>Our Test Setup:
<ul data-start=”1210″ data-end=”1682″><strong data-start=”1212″ data-end=”1220″>Ball: 83 mm smooth solid steel ball, 2.3 kg
<strong data-start=”1262″ data-end=”1277″>Drop Height: 3.66 m (12 ft ± 5 in)
<strong data-start=”1303″ data-end=”1325″>Glass Conditioning: 4+ hours at 24°C ± 5°C
<strong data-start=”1352″ data-end=”1369″>Support Frame: Matches general F3007 frame design (though possibly not identical to lab’s)
<strong data-start=”1449″ data-end=”1461″>Clamping: We try not to over-clamp, but may be tighter than the lab
<strong data-start=”1523″ data-end=”1542″>Glass Thickness: Testing the thinnest configuration per production batch
<strong data-start=”1602″ data-end=”1615″>Test Spec: ASTM F3007, not CPSC 16 CFR 1201 (we know CPSC uses a 100 lb bag)
<hr data-start=”1684″ data-end=”1687″>
<b data-start=”1689″ data-end=”1721″>Theories We’re Exploring:-
<strong data-start=”1726″ data-end=”1768″>Improper drop frame/ball release setup – might not be a true free fall?
-
<strong data-start=”1805″ data-end=”1833″>Slightly off drop height (we’ve measured but rechecking for precision).
-
<strong data-start=”1884″ data-end=”1912″>Over-clamping the sample – maybe creating excessive edge stress. We currently barely clamp it so I don’t think it can be this.
-
<strong data-start=”1956″ data-end=”1989″>Differences in ball condition – is surface wear causing inconsistency?
-
<strong data-start=”2034″ data-end=”2059″>Environmental factors – conditioning room vs test area temperature/humidity?
<hr data-start=”2199″ data-end=”2202″>
<b data-start=”2204″ data-end=”2238″>Question for the Community:Has anyone else experienced this kind of <strong data-start=”2281″ data-end=”2358″>inconsistency between certified lab tests and in-house ball drop failures under SGCC/ASTM F3007 procedures?
Would love to hear:
<ul data-start=”2414″ data-end=”2733″>
What kind of <strong data-start=”2429″ data-end=”2443″>drop setup you’re using (custom-built vs purchased system)
Any tricks you’ve found helpful when <strong data-start=”2531″ data-end=”2569″>calibrating drop height or release
How you handle <strong data-start=”2587″ data-end=”2607″>clamping/support without creating non-representative stress
Whether your <strong data-start=”2666″ data-end=”2692″>ball surface condition or <strong data-start=”2696″ data-end=”2715″>support backing has caused issues
Really appreciate any input — we’re committed to dialing this in and avoiding false failures (or worse, missing a real one).
Sorry, there were no replies found.
Log in to reply.